Galvanic corrosion of molybdenum alloys and oxides in contact with copper for thin film transistors using evans diagrams

Research output: Contribution to journalConference articlepeer-review

Standard

Galvanic corrosion of molybdenum alloys and oxides in contact with copper for thin film transistors using evans diagrams. / Riedl, Jessica; Mori, Gregor; Schmidt, Hennrik et al.
In: Digest of technical papers, Vol. 52, No. S2, 2021, p. 588-590.

Research output: Contribution to journalConference articlepeer-review

Bibtex - Download

@article{6cd7470076924d9091642a3e2f495a68,
title = "Galvanic corrosion of molybdenum alloys and oxides in contact with copper for thin film transistors using evans diagrams",
keywords = "Evans diagram, Galvanic corrosion, Mo alloys, Mo oxides, TFTs",
author = "Jessica Riedl and Gregor Mori and Hennrik Schmidt and Harald K{\"o}stenbauer",
note = "Publisher Copyright: {\textcopyright} 2021, John Wiley and Sons Inc. All rights reserved.; International Conference on Display Technology, ICDT 2021 ; Conference date: 30-05-2021 Through 02-06-2021",
year = "2021",
doi = "10.1002/sdtp.15212",
language = "English",
volume = "52",
pages = "588--590",
journal = "Digest of technical papers",
issn = "0082-0830",
number = "S2",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Galvanic corrosion of molybdenum alloys and oxides in contact with copper for thin film transistors using evans diagrams

AU - Riedl, Jessica

AU - Mori, Gregor

AU - Schmidt, Hennrik

AU - Köstenbauer, Harald

N1 - Publisher Copyright: © 2021, John Wiley and Sons Inc. All rights reserved.

PY - 2021

Y1 - 2021

KW - Evans diagram

KW - Galvanic corrosion

KW - Mo alloys

KW - Mo oxides

KW - TFTs

UR - http://www.scopus.com/inward/record.url?scp=85115842786&partnerID=8YFLogxK

U2 - 10.1002/sdtp.15212

DO - 10.1002/sdtp.15212

M3 - Conference article

AN - SCOPUS:85115842786

VL - 52

SP - 588

EP - 590

JO - Digest of technical papers

JF - Digest of technical papers

SN - 0082-0830

IS - S2

T2 - International Conference on Display Technology, ICDT 2021

Y2 - 30 May 2021 through 2 June 2021

ER -