Galvanic corrosion of molybdenum alloys and oxides in contact with copper for thin film transistors using evans diagrams
Publikationen: Beitrag in Fachzeitschrift › Konferenzartikel › (peer-reviewed)
Standard
in: Digest of technical papers, Jahrgang 52, Nr. S2, 2021, S. 588-590.
Publikationen: Beitrag in Fachzeitschrift › Konferenzartikel › (peer-reviewed)
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Galvanic corrosion of molybdenum alloys and oxides in contact with copper for thin film transistors using evans diagrams
AU - Riedl, Jessica
AU - Mori, Gregor
AU - Schmidt, Hennrik
AU - Köstenbauer, Harald
N1 - Publisher Copyright: © 2021, John Wiley and Sons Inc. All rights reserved.
PY - 2021
Y1 - 2021
KW - Evans diagram
KW - Galvanic corrosion
KW - Mo alloys
KW - Mo oxides
KW - TFTs
UR - http://www.scopus.com/inward/record.url?scp=85115842786&partnerID=8YFLogxK
U2 - 10.1002/sdtp.15212
DO - 10.1002/sdtp.15212
M3 - Conference article
AN - SCOPUS:85115842786
VL - 52
SP - 588
EP - 590
JO - Digest of technical papers
JF - Digest of technical papers
SN - 0082-0830
IS - S2
T2 - International Conference on Display Technology, ICDT 2021
Y2 - 30 May 2021 through 2 June 2021
ER -