Does dynamic nanoindentation testing influence the acquired mechanical properties?

Research output: Contribution to conferencePresentationResearch

Standard

Does dynamic nanoindentation testing influence the acquired mechanical properties? / Leitner, Alexander; Cordill, Megan J; Maier-Kiener, Verena et al.
2016. 2016 MRS Fall Meeting & Exhibit, Boston, United States.

Research output: Contribution to conferencePresentationResearch

Harvard

Bibtex - Download

@conference{ce15752853734656b7406deec1b15e18,
title = "Does dynamic nanoindentation testing influence the acquired mechanical properties?",
author = "Alexander Leitner and Cordill, {Megan J} and Verena Maier-Kiener and Daniel Kiener",
year = "2016",
language = "English",
note = "2016 MRS Fall Meeting & Exhibit ; Conference date: 27-11-2016 Through 02-12-2016",

}

RIS (suitable for import to EndNote) - Download

TY - CONF

T1 - Does dynamic nanoindentation testing influence the acquired mechanical properties?

AU - Leitner, Alexander

AU - Cordill, Megan J

AU - Maier-Kiener, Verena

AU - Kiener, Daniel

PY - 2016

Y1 - 2016

M3 - Presentation

T2 - 2016 MRS Fall Meeting & Exhibit

Y2 - 27 November 2016 through 2 December 2016

ER -