Does dynamic nanoindentation testing influence the acquired mechanical properties?
Publikationen: Konferenzbeitrag › Vortrag › Forschung
Standard
Does dynamic nanoindentation testing influence the acquired mechanical properties? / Leitner, Alexander; Cordill, Megan J; Maier-Kiener, Verena et al.
2016. 2016 MRS Fall Meeting & Exhibit, Boston, USA / Vereinigte Staaten.
2016. 2016 MRS Fall Meeting & Exhibit, Boston, USA / Vereinigte Staaten.
Publikationen: Konferenzbeitrag › Vortrag › Forschung
Harvard
Leitner, A, Cordill, MJ, Maier-Kiener, V & Kiener, D 2016, 'Does dynamic nanoindentation testing influence the acquired mechanical properties?', 2016 MRS Fall Meeting & Exhibit, Boston, USA / Vereinigte Staaten, 27/11/16 - 2/12/16.
APA
Leitner, A., Cordill, M. J., Maier-Kiener, V., & Kiener, D. (2016). Does dynamic nanoindentation testing influence the acquired mechanical properties?. 2016 MRS Fall Meeting & Exhibit, Boston, USA / Vereinigte Staaten.
Vancouver
Leitner A, Cordill MJ, Maier-Kiener V, Kiener D. Does dynamic nanoindentation testing influence the acquired mechanical properties?. 2016. 2016 MRS Fall Meeting & Exhibit, Boston, USA / Vereinigte Staaten.
Author
Bibtex - Download
@conference{ce15752853734656b7406deec1b15e18,
title = "Does dynamic nanoindentation testing influence the acquired mechanical properties?",
author = "Alexander Leitner and Cordill, {Megan J} and Verena Maier-Kiener and Daniel Kiener",
year = "2016",
language = "English",
note = "2016 MRS Fall Meeting & Exhibit ; Conference date: 27-11-2016 Through 02-12-2016",
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - Does dynamic nanoindentation testing influence the acquired mechanical properties?
AU - Leitner, Alexander
AU - Cordill, Megan J
AU - Maier-Kiener, Verena
AU - Kiener, Daniel
PY - 2016
Y1 - 2016
M3 - Presentation
T2 - 2016 MRS Fall Meeting & Exhibit
Y2 - 27 November 2016 through 2 December 2016
ER -