Does dynamic nanoindentation testing influence the acquired mechanical properties?
Research output: Contribution to conference › Presentation › Research
Authors
Organisational units
Details
Original language | English |
---|---|
Publication status | Published - 2016 |
Event | 2016 MRS Fall Meeting & Exhibit - Boston, United States Duration: 27 Nov 2016 → 2 Dec 2016 |
Conference
Conference | 2016 MRS Fall Meeting & Exhibit |
---|---|
Country/Territory | United States |
City | Boston |
Period | 27/11/16 → 2/12/16 |