Correlative microstructure and topography informed nanoindentation of copper films

Research output: Contribution to journalArticleResearchpeer-review

Organisational units

External Organisational units

  • Erich Schmid Institute of Materials Science

Details

Original languageEnglish
Pages (from-to)404-413
Number of pages10
JournalSurface & coatings technology
Volume308.2016
Issue number25 December
DOIs