Nanoindentation in Teeth: The Influence of Experimental Conditions on local mechanical Properties

Research output: Contribution to conferencePosterResearchpeer-review

Standard

Nanoindentation in Teeth: The Influence of Experimental Conditions on local mechanical Properties. / Guidoni, Griselda-Maria; Denkmayr, J.; Schöberl, Thomas et al.
2005. Poster session presented at Instrumented Indentation Testing in Materials Research and Development, Kreta, Griechenland.

Research output: Contribution to conferencePosterResearchpeer-review

Harvard

Guidoni, G-M, Denkmayr, J, Schöberl, T & Jäger, I 2005, 'Nanoindentation in Teeth: The Influence of Experimental Conditions on local mechanical Properties', Instrumented Indentation Testing in Materials Research and Development, Kreta, Griechenland, 9/10/05 - 14/10/05.

APA

Guidoni, G.-M., Denkmayr, J., Schöberl, T., & Jäger, I. (2005). Nanoindentation in Teeth: The Influence of Experimental Conditions on local mechanical Properties. Poster session presented at Instrumented Indentation Testing in Materials Research and Development, Kreta, Griechenland.

Vancouver

Guidoni GM, Denkmayr J, Schöberl T, Jäger I. Nanoindentation in Teeth: The Influence of Experimental Conditions on local mechanical Properties. 2005. Poster session presented at Instrumented Indentation Testing in Materials Research and Development, Kreta, Griechenland.

Author

Guidoni, Griselda-Maria ; Denkmayr, J. ; Schöberl, Thomas et al. / Nanoindentation in Teeth: The Influence of Experimental Conditions on local mechanical Properties. Poster session presented at Instrumented Indentation Testing in Materials Research and Development, Kreta, Griechenland.

Bibtex - Download

@conference{dc98b259414b4dd1a10b0f5808767cc4,
title = "Nanoindentation in Teeth: The Influence of Experimental Conditions on local mechanical Properties",
author = "Griselda-Maria Guidoni and J. Denkmayr and Thomas Sch{\"o}berl and Ingomar J{\"a}ger",
year = "2005",
language = "English",
note = "Instrumented Indentation Testing in Materials Research and Development ; Conference date: 09-10-2005 Through 14-10-2005",

}

RIS (suitable for import to EndNote) - Download

TY - CONF

T1 - Nanoindentation in Teeth: The Influence of Experimental Conditions on local mechanical Properties

AU - Guidoni, Griselda-Maria

AU - Denkmayr, J.

AU - Schöberl, Thomas

AU - Jäger, Ingomar

PY - 2005

Y1 - 2005

M3 - Poster

T2 - Instrumented Indentation Testing in Materials Research and Development

Y2 - 9 October 2005 through 14 October 2005

ER -