Nanoindentation of wet and dry compact bone: Influence of environment and indenter tip geometry on the indentation modulus

Research output: Contribution to journalArticleResearchpeer-review

Authors

Organisational units

Details

Translated title of the contributionNanoindentation of wet and dry compact bone: Influence of environment and indenter tip geometry on the indentation modulus
Original languageEnglish
Pages (from-to)553-565
JournalPhilosophical magazine
Publication statusPublished - 2010