Mechanical properties of spruce wood cell walls by nanoindentation

Research output: Contribution to journalArticleResearchpeer-review

Standard

Mechanical properties of spruce wood cell walls by nanoindentation. / Gindl, W.; Gupta, H. S.; Schöberl, Thomas et al.
In: Applied physics / A (Series A, Materials science & processing), Vol. 79, 2004, p. 2069-2073.

Research output: Contribution to journalArticleResearchpeer-review

Harvard

Gindl, W, Gupta, HS, Schöberl, T, Lichtenegger, HC & Fratzl, P 2004, 'Mechanical properties of spruce wood cell walls by nanoindentation', Applied physics / A (Series A, Materials science & processing), vol. 79, pp. 2069-2073.

APA

Gindl, W., Gupta, H. S., Schöberl, T., Lichtenegger, H. C., & Fratzl, P. (2004). Mechanical properties of spruce wood cell walls by nanoindentation. Applied physics / A (Series A, Materials science & processing), 79, 2069-2073.

Vancouver

Author

Gindl, W. ; Gupta, H. S. ; Schöberl, Thomas et al. / Mechanical properties of spruce wood cell walls by nanoindentation. In: Applied physics / A (Series A, Materials science & processing). 2004 ; Vol. 79. pp. 2069-2073.

Bibtex - Download

@article{0f8851d09b4d4f98ab4367cd6828bef0,
title = "Mechanical properties of spruce wood cell walls by nanoindentation",
author = "W. Gindl and Gupta, {H. S.} and Thomas Sch{\"o}berl and Lichtenegger, {H. C.} and P. Fratzl",
year = "2004",
language = "English",
volume = "79",
pages = "2069--2073",
journal = "Applied physics / A (Series A, Materials science & processing)",
issn = "0340-3793",
publisher = "Springer Berlin",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Mechanical properties of spruce wood cell walls by nanoindentation

AU - Gindl, W.

AU - Gupta, H. S.

AU - Schöberl, Thomas

AU - Lichtenegger, H. C.

AU - Fratzl, P.

PY - 2004

Y1 - 2004

M3 - Article

VL - 79

SP - 2069

EP - 2073

JO - Applied physics / A (Series A, Materials science & processing)

JF - Applied physics / A (Series A, Materials science & processing)

SN - 0340-3793

ER -