Mechanical properties of spruce wood cell walls by nanoindentation
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Standard
Mechanical properties of spruce wood cell walls by nanoindentation. / Gindl, W.; Gupta, H. S.; Schöberl, Thomas et al.
in: Applied physics / A (Series A, Materials science & processing), Jahrgang 79, 2004, S. 2069-2073.
in: Applied physics / A (Series A, Materials science & processing), Jahrgang 79, 2004, S. 2069-2073.
Publikationen: Beitrag in Fachzeitschrift › Artikel › Forschung › (peer-reviewed)
Harvard
Gindl, W, Gupta, HS, Schöberl, T, Lichtenegger, HC & Fratzl, P 2004, 'Mechanical properties of spruce wood cell walls by nanoindentation', Applied physics / A (Series A, Materials science & processing), Jg. 79, S. 2069-2073.
APA
Gindl, W., Gupta, H. S., Schöberl, T., Lichtenegger, H. C., & Fratzl, P. (2004). Mechanical properties of spruce wood cell walls by nanoindentation. Applied physics / A (Series A, Materials science & processing), 79, 2069-2073.
Vancouver
Gindl W, Gupta HS, Schöberl T, Lichtenegger HC, Fratzl P. Mechanical properties of spruce wood cell walls by nanoindentation. Applied physics / A (Series A, Materials science & processing). 2004;79:2069-2073.
Author
Bibtex - Download
@article{0f8851d09b4d4f98ab4367cd6828bef0,
title = "Mechanical properties of spruce wood cell walls by nanoindentation",
author = "W. Gindl and Gupta, {H. S.} and Thomas Sch{\"o}berl and Lichtenegger, {H. C.} and P. Fratzl",
year = "2004",
language = "English",
volume = "79",
pages = "2069--2073",
journal = "Applied physics / A (Series A, Materials science & processing)",
issn = "0340-3793",
publisher = "Springer Berlin",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Mechanical properties of spruce wood cell walls by nanoindentation
AU - Gindl, W.
AU - Gupta, H. S.
AU - Schöberl, Thomas
AU - Lichtenegger, H. C.
AU - Fratzl, P.
PY - 2004
Y1 - 2004
M3 - Article
VL - 79
SP - 2069
EP - 2073
JO - Applied physics / A (Series A, Materials science & processing)
JF - Applied physics / A (Series A, Materials science & processing)
SN - 0340-3793
ER -