In-situ Observation of Cross- Sectional Microstructural Changes and Stress Distributions in Fracturing TiN Thin Film during Nanoindentation
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
External Organisational units
- University of Kiel and Helmholtz Zentrum Geesthacht
- Materials Center Leoben Forschungs GmbH
Details
Original language | English |
---|---|
Pages (from-to) | 1-14 |
Number of pages | 14 |
Journal | Scientific reports (London : Nature Publishing Group) |
Volume | 6:22670 |
DOIs | |
Publication status | Published - 7 Mar 2016 |