Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Standard

Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91. / Gerstmayr, Gerhard; Mori, Gregor; Eichlseder, Wilfried.
Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition. 2010. p. 145-150 (Magnesium Technology).

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Harvard

Gerstmayr, G, Mori, G & Eichlseder, W 2010, Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91. in Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition. Magnesium Technology, pp. 145-150, Magnesium Technology 2010 - TMS 2010 Annual Meeting and Exhibition, Seattle, WA, United States, 14/02/10.

APA

Gerstmayr, G., Mori, G., & Eichlseder, W. (2010). Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91. In Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition (pp. 145-150). (Magnesium Technology).

Vancouver

Gerstmayr G, Mori G, Eichlseder W. Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91. In Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition. 2010. p. 145-150. (Magnesium Technology).

Author

Gerstmayr, Gerhard ; Mori, Gregor ; Eichlseder, Wilfried. / Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91. Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition. 2010. pp. 145-150 (Magnesium Technology).

Bibtex - Download

@inproceedings{547e1219ef3c4481b00e7f0add09cada,
title = "Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91",
keywords = "Galvanic corrosion, High-strength aluminum bolt, Magnesium, Stress corrosion cracking",
author = "Gerhard Gerstmayr and Gregor Mori and Wilfried Eichlseder",
year = "2010",
month = may,
day = "21",
language = "English",
isbn = "9780873397469",
series = "Magnesium Technology",
pages = "145--150",
booktitle = "Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition",
note = "Magnesium Technology 2010 - TMS 2010 Annual Meeting and Exhibition ; Conference date: 14-02-2010 Through 18-02-2010",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91

AU - Gerstmayr, Gerhard

AU - Mori, Gregor

AU - Eichlseder, Wilfried

PY - 2010/5/21

Y1 - 2010/5/21

KW - Galvanic corrosion

KW - High-strength aluminum bolt

KW - Magnesium

KW - Stress corrosion cracking

UR - http://www.scopus.com/inward/record.url?scp=77952330271&partnerID=8YFLogxK

M3 - Conference contribution

AN - SCOPUS:77952330271

SN - 9780873397469

T3 - Magnesium Technology

SP - 145

EP - 150

BT - Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition

T2 - Magnesium Technology 2010 - TMS 2010 Annual Meeting and Exhibition

Y2 - 14 February 2010 through 18 February 2010

ER -