Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Standard
Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition. 2010. S. 145-150 (Magnesium Technology).
Publikationen: Beitrag in Buch/Bericht/Konferenzband › Beitrag in Konferenzband
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - GEN
T1 - Galvanic corrosion and stress corrosion cracking of steel and aluminum bolts in magnesium die cast alloy AZ91
AU - Gerstmayr, Gerhard
AU - Mori, Gregor
AU - Eichlseder, Wilfried
PY - 2010/5/21
Y1 - 2010/5/21
KW - Galvanic corrosion
KW - High-strength aluminum bolt
KW - Magnesium
KW - Stress corrosion cracking
UR - http://www.scopus.com/inward/record.url?scp=77952330271&partnerID=8YFLogxK
M3 - Conference contribution
AN - SCOPUS:77952330271
SN - 9780873397469
T3 - Magnesium Technology
SP - 145
EP - 150
BT - Magnesium Technology 2010 - Held During TMS 2010 Annual Meeting and Exhibition
T2 - Magnesium Technology 2010 - TMS 2010 Annual Meeting and Exhibition
Y2 - 14 February 2010 through 18 February 2010
ER -