Finite Element Simulation of the Effect of surface roughness on nanoindentation of thin films with spherical indenters
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
Details
Translated title of the contribution | Finite Element Simulation of the Effect of surface roughness on nanoindentation of thin films with spherical indenters |
---|---|
Original language | English |
Pages (from-to) | 1103-1107 |
Journal | Surface & coatings technology |
Volume | 202 |
Publication status | Published - 2007 |