Finite Element Simulation of the Effect of surface roughness on nanoindentation of thin films with spherical indenters
Research output: Contribution to journal › Article › Research › peer-review
Standard
Finite Element Simulation of the Effect of surface roughness on nanoindentation of thin films with spherical indenters. / Walter, Claudia; Antretter, Thomas; Daniel, Rostislav et al.
In: Surface & coatings technology, Vol. 202, 2007, p. 1103-1107.
In: Surface & coatings technology, Vol. 202, 2007, p. 1103-1107.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
APA
Vancouver
Author
Bibtex - Download
@article{bbce21db9f36471e83fc9f49b079cb8a,
title = "Finite Element Simulation of the Effect of surface roughness on nanoindentation of thin films with spherical indenters",
author = "Claudia Walter and Thomas Antretter and Rostislav Daniel and Christian Mitterer",
year = "2007",
language = "English",
volume = "202",
pages = "1103--1107",
journal = "Surface & coatings technology",
issn = "0257-8972",
publisher = "Elsevier",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Finite Element Simulation of the Effect of surface roughness on nanoindentation of thin films with spherical indenters
AU - Walter, Claudia
AU - Antretter, Thomas
AU - Daniel, Rostislav
AU - Mitterer, Christian
PY - 2007
Y1 - 2007
M3 - Article
VL - 202
SP - 1103
EP - 1107
JO - Surface & coatings technology
JF - Surface & coatings technology
SN - 0257-8972
ER -