Discrete dislocation simulation of nanoindentation: the effect of moving conditions and indenter shape
Research output: Contribution to journal › Article › Research › peer-review
Standard
In: Materials science and engineering: A, Structural materials: properties, microstructure and processing, Vol. 387-389, 2004, p. 254-256.