Discrete dislocation simulation of nanoindentation: the effect of moving conditions and indenter shape

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

Discrete dislocation simulation of nanoindentation: the effect of moving conditions and indenter shape. / Kreuzer, H. G. M.; Pippan, Reinhard.
in: Materials science and engineering: A, Structural materials: properties, microstructure and processing, Jahrgang 387-389, 2004, S. 254-256.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Bibtex - Download

@article{00db820517b54b73b8d55cd2adca2409,
title = "Discrete dislocation simulation of nanoindentation: the effect of moving conditions and indenter shape",
author = "Kreuzer, {H. G. M.} and Reinhard Pippan",
year = "2004",
language = "English",
volume = "387-389",
pages = "254--256",
journal = "Materials science and engineering: A, Structural materials: properties, microstructure and processing",
issn = "0921-5093",
publisher = "Elsevier",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Discrete dislocation simulation of nanoindentation: the effect of moving conditions and indenter shape

AU - Kreuzer, H. G. M.

AU - Pippan, Reinhard

PY - 2004

Y1 - 2004

M3 - Article

VL - 387-389

SP - 254

EP - 256

JO - Materials science and engineering: A, Structural materials: properties, microstructure and processing

JF - Materials science and engineering: A, Structural materials: properties, microstructure and processing

SN - 0921-5093

ER -