Development of a device and method for fractographic investigations of refractories
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Authors
Organisational units
Details
Translated title of the contribution | Development of a device and method for fractographic investigations of refractories |
---|---|
Original language | English |
Title of host publication | Unified International technical Conference on Refractories UNITECR'07 |
Pages | 494-497 |