Fractographic investigation of refractories

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Organisational units

Details

Translated title of the contributionFractographic investigation of refractories
Original languageEnglish
Title of host publicationUNITECR 2009 Summary Booklet
Pages26-26
Publication statusPublished - 2009