Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
External Organisational units
- Xi'an University of Technology
Details
Original language | English |
---|---|
Pages (from-to) | 581-590 |
Number of pages | 10 |
Journal | Journal of alloys and compounds |
Volume | 699.2017 |
Issue number | 30 March |