Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures
Research output: Contribution to journal › Article › Research › peer-review
Standard
Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures. / Liu, Jun; Tang, Wenting; Li, Jiehua.
In: Journal of alloys and compounds, Vol. 699.2017, No. 30 March, 26.12.2016, p. 581-590.
In: Journal of alloys and compounds, Vol. 699.2017, No. 30 March, 26.12.2016, p. 581-590.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
Liu, J, Tang, W & Li, J 2016, 'Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures', Journal of alloys and compounds, vol. 699.2017, no. 30 March, pp. 581-590. https://doi.org/10.1016/j.jallcom.2016.12.325
APA
Liu, J., Tang, W., & Li, J. (2016). Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures. Journal of alloys and compounds, 699.2017(30 March), 581-590. https://doi.org/10.1016/j.jallcom.2016.12.325
Vancouver
Liu J, Tang W, Li J. Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures. Journal of alloys and compounds. 2016 Dec 26;699.2017(30 March):581-590. doi: 10.1016/j.jallcom.2016.12.325
Author
Bibtex - Download
@article{1e2980ef147b4d9497069220adafd0d6,
title = "Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures",
author = "Jun Liu and Wenting Tang and Jiehua Li",
year = "2016",
month = dec,
day = "26",
doi = "10.1016/j.jallcom.2016.12.325",
language = "English",
volume = "699.2017",
pages = "581--590",
journal = "Journal of alloys and compounds",
issn = "0925-8388",
publisher = "Elsevier",
number = "30 March",
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Deformation and fracture behaviors of K403 Ni-based superalloy at elevated temperatures
AU - Liu, Jun
AU - Tang, Wenting
AU - Li, Jiehua
PY - 2016/12/26
Y1 - 2016/12/26
U2 - 10.1016/j.jallcom.2016.12.325
DO - 10.1016/j.jallcom.2016.12.325
M3 - Article
VL - 699.2017
SP - 581
EP - 590
JO - Journal of alloys and compounds
JF - Journal of alloys and compounds
SN - 0925-8388
IS - 30 March
ER -