Combined theoretical and experimental study of Fe-Al-Ti superalloys
Research output: Contribution to conference › Poster › Research
Standard
Combined theoretical and experimental study of Fe-Al-Ti superalloys. / Friák, Martin; Miháliková, Ivana; Slávik, Anton et al.
2018. Poster session presented at TYC 5th Energy Workshop, London, United Kingdom.
2018. Poster session presented at TYC 5th Energy Workshop, London, United Kingdom.
Research output: Contribution to conference › Poster › Research
Harvard
Friák, M, Miháliková, I, Slávik, A, Homola, V, Bursikova, V, Pizurová, N, Pavlu, J, Dymacek, P, Dobes, F, Holec, D, Koutná, N, Jiraskova, Y & Šob, M 2018, 'Combined theoretical and experimental study of Fe-Al-Ti superalloys', TYC 5th Energy Workshop, London, United Kingdom, 25/07/18 - 27/07/18.
APA
Friák, M., Miháliková, I., Slávik, A., Homola, V., Bursikova, V., Pizurová, N., Pavlu, J., Dymacek, P., Dobes, F., Holec, D., Koutná, N., Jiraskova, Y., & Šob, M. (2018). Combined theoretical and experimental study of Fe-Al-Ti superalloys. Poster session presented at TYC 5th Energy Workshop, London, United Kingdom.
Vancouver
Friák M, Miháliková I, Slávik A, Homola V, Bursikova V, Pizurová N et al.. Combined theoretical and experimental study of Fe-Al-Ti superalloys. 2018. Poster session presented at TYC 5th Energy Workshop, London, United Kingdom.
Author
Bibtex - Download
@conference{b4fe85e2a36c49eb897a2e88d967f70f,
title = "Combined theoretical and experimental study of Fe-Al-Ti superalloys",
author = "Martin Fri{\'a}k and Ivana Mih{\'a}likov{\'a} and Anton Sl{\'a}vik and Vojtech Homola and Vilma Bursikova and Nadezda Pizurov{\'a} and Jana Pavlu and Petr Dymacek and Ferdinand Dobes and David Holec and Nikola Koutn{\'a} and Yvonna Jiraskova and Mojm{\'i}r {\v S}ob",
year = "2018",
language = "English",
note = "TYC 5th Energy Workshop ; Conference date: 25-07-2018 Through 27-07-2018",
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - Combined theoretical and experimental study of Fe-Al-Ti superalloys
AU - Friák, Martin
AU - Miháliková, Ivana
AU - Slávik, Anton
AU - Homola, Vojtech
AU - Bursikova, Vilma
AU - Pizurová, Nadezda
AU - Pavlu, Jana
AU - Dymacek, Petr
AU - Dobes, Ferdinand
AU - Holec, David
AU - Koutná, Nikola
AU - Jiraskova, Yvonna
AU - Šob, Mojmír
PY - 2018
Y1 - 2018
M3 - Poster
T2 - TYC 5th Energy Workshop
Y2 - 25 July 2018 through 27 July 2018
ER -