Combined theoretical and experimental study of Fe-Al-Ti superalloys

Publikationen: KonferenzbeitragPosterForschung

Standard

Combined theoretical and experimental study of Fe-Al-Ti superalloys. / Friák, Martin; Miháliková, Ivana; Slávik, Anton et al.
2018. Postersitzung präsentiert bei TYC 5th Energy Workshop, London, Großbritannien / Vereinigtes Königreich.

Publikationen: KonferenzbeitragPosterForschung

Harvard

Friák, M, Miháliková, I, Slávik, A, Homola, V, Bursikova, V, Pizurová, N, Pavlu, J, Dymacek, P, Dobes, F, Holec, D, Koutná, N, Jiraskova, Y & Šob, M 2018, 'Combined theoretical and experimental study of Fe-Al-Ti superalloys', TYC 5th Energy Workshop, London, Großbritannien / Vereinigtes Königreich, 25/07/18 - 27/07/18.

APA

Friák, M., Miháliková, I., Slávik, A., Homola, V., Bursikova, V., Pizurová, N., Pavlu, J., Dymacek, P., Dobes, F., Holec, D., Koutná, N., Jiraskova, Y., & Šob, M. (2018). Combined theoretical and experimental study of Fe-Al-Ti superalloys. Postersitzung präsentiert bei TYC 5th Energy Workshop, London, Großbritannien / Vereinigtes Königreich.

Vancouver

Friák M, Miháliková I, Slávik A, Homola V, Bursikova V, Pizurová N et al.. Combined theoretical and experimental study of Fe-Al-Ti superalloys. 2018. Postersitzung präsentiert bei TYC 5th Energy Workshop, London, Großbritannien / Vereinigtes Königreich.

Author

Friák, Martin ; Miháliková, Ivana ; Slávik, Anton et al. / Combined theoretical and experimental study of Fe-Al-Ti superalloys. Postersitzung präsentiert bei TYC 5th Energy Workshop, London, Großbritannien / Vereinigtes Königreich.

Bibtex - Download

@conference{b4fe85e2a36c49eb897a2e88d967f70f,
title = "Combined theoretical and experimental study of Fe-Al-Ti superalloys",
author = "Martin Fri{\'a}k and Ivana Mih{\'a}likov{\'a} and Anton Sl{\'a}vik and Vojtech Homola and Vilma Bursikova and Nadezda Pizurov{\'a} and Jana Pavlu and Petr Dymacek and Ferdinand Dobes and David Holec and Nikola Koutn{\'a} and Yvonna Jiraskova and Mojm{\'i}r {\v S}ob",
year = "2018",
language = "English",
note = "TYC 5th Energy Workshop ; Conference date: 25-07-2018 Through 27-07-2018",

}

RIS (suitable for import to EndNote) - Download

TY - CONF

T1 - Combined theoretical and experimental study of Fe-Al-Ti superalloys

AU - Friák, Martin

AU - Miháliková, Ivana

AU - Slávik, Anton

AU - Homola, Vojtech

AU - Bursikova, Vilma

AU - Pizurová, Nadezda

AU - Pavlu, Jana

AU - Dymacek, Petr

AU - Dobes, Ferdinand

AU - Holec, David

AU - Koutná, Nikola

AU - Jiraskova, Yvonna

AU - Šob, Mojmír

PY - 2018

Y1 - 2018

M3 - Poster

T2 - TYC 5th Energy Workshop

Y2 - 25 July 2018 through 27 July 2018

ER -