Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Standard
International Corrosion Conference series / National Association of Corrosion Engineers: Corrosion 2002. Vol. 2002-April 2002. (NACE - International Corrosion Conference Series).
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - GEN
T1 - Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant
AU - Mori, G.
AU - Zitter, H.
AU - Maurer, Karl L.
PY - 2002/1/1
Y1 - 2002/1/1
KW - Failure
KW - Heat exchanger
KW - Pitting corrosion
KW - Pulp industry
KW - Stainless steel
KW - Stress corrosion cracking
KW - Temperature concentration stability diagrams
KW - X2CrNiMo18-14-3
UR - http://www.scopus.com/inward/record.url?scp=84865428019&partnerID=8YFLogxK
M3 - Conference contribution
AN - SCOPUS:84865428019
VL - 2002-April
T3 - NACE - International Corrosion Conference Series
BT - International Corrosion Conference series / National Association of Corrosion Engineers
T2 - Corrosion 2002
Y2 - 7 April 2002 through 11 April 2002
ER -