Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Konferenzband

Standard

Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant. / Mori, G.; Zitter, H.; Maurer, Karl L.
International Corrosion Conference series / National Association of Corrosion Engineers: Corrosion 2002. Band 2002-April 2002. (NACE - International Corrosion Conference Series).

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Konferenzband

Harvard

Mori, G, Zitter, H & Maurer, KL 2002, Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant. in International Corrosion Conference series / National Association of Corrosion Engineers: Corrosion 2002. Bd. 2002-April, NACE - International Corrosion Conference Series, Corrosion 2002, Denver, USA / Vereinigte Staaten, 7/04/02.

APA

Mori, G., Zitter, H., & Maurer, K. L. (2002). Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant. In International Corrosion Conference series / National Association of Corrosion Engineers: Corrosion 2002 (Band 2002-April). (NACE - International Corrosion Conference Series).

Vancouver

Mori G, Zitter H, Maurer KL. Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant. in International Corrosion Conference series / National Association of Corrosion Engineers: Corrosion 2002. Band 2002-April. 2002. (NACE - International Corrosion Conference Series).

Author

Mori, G. ; Zitter, H. ; Maurer, Karl L. / Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant. International Corrosion Conference series / National Association of Corrosion Engineers: Corrosion 2002. Band 2002-April 2002. (NACE - International Corrosion Conference Series).

Bibtex - Download

@inproceedings{1ab5d0f6127749c3bfae4d6b55901066,
title = "Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant",
keywords = "Failure, Heat exchanger, Pitting corrosion, Pulp industry, Stainless steel, Stress corrosion cracking, Temperature concentration stability diagrams, X2CrNiMo18-14-3",
author = "G. Mori and H. Zitter and Maurer, {Karl L.}",
year = "2002",
month = jan,
day = "1",
language = "English",
volume = "2002-April",
series = "NACE - International Corrosion Conference Series",
booktitle = "International Corrosion Conference series / National Association of Corrosion Engineers",
note = "Corrosion 2002 ; Conference date: 07-04-2002 Through 11-04-2002",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - Chloride induced stress corrosion cracking and pitting corrosion of a stainless steel X2CrNiMo18-14-3 heat exchanger of a pulp plant

AU - Mori, G.

AU - Zitter, H.

AU - Maurer, Karl L.

PY - 2002/1/1

Y1 - 2002/1/1

KW - Failure

KW - Heat exchanger

KW - Pitting corrosion

KW - Pulp industry

KW - Stainless steel

KW - Stress corrosion cracking

KW - Temperature concentration stability diagrams

KW - X2CrNiMo18-14-3

UR - http://www.scopus.com/inward/record.url?scp=84865428019&partnerID=8YFLogxK

M3 - Conference contribution

AN - SCOPUS:84865428019

VL - 2002-April

T3 - NACE - International Corrosion Conference Series

BT - International Corrosion Conference series / National Association of Corrosion Engineers

T2 - Corrosion 2002

Y2 - 7 April 2002 through 11 April 2002

ER -