On the systematic investigation of acicular ferrite on laboratory scale
Publikationen: Thesis / Studienabschlussarbeiten und Habilitationsschriften › Dissertation
Standard
2016.
Publikationen: Thesis / Studienabschlussarbeiten und Habilitationsschriften › Dissertation
Harvard
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - BOOK
T1 - On the systematic investigation of acicular ferrite on laboratory scale
AU - Loder, Denise
N1 - no embargo
PY - 2016
Y1 - 2016
N2 - Acicular ferrite nucleates intragranularly on non-metallic inclusions, forming an arrangement of fine, interlocking grains. This characteristic structure is known to improve the steel toughness significantly, what makes acicular ferrite of increasing interest to steel producers. However, the formation of acicular ferrite is still not completely clarified. Therefore, the present thesis developed a holistic and systematic methodology to study the acicular ferrite formation and its influencing factors on laboratory scale. First, the necessary steel composition to create a desired inclusion landscape is determined by thermodynamic calculations using FactSage. Second, samples with defined and homogenously distributed inclusions are produced by melting experiments in a Tammann type furnace. The methodology only uses endogenous inclusions, resulting from deoxidation and desulphurization, as nucleation sites for acicular ferrite, so that the steel cleanness is not deteriorated artificially by the addition of synthetic particles. Third, the samples are heat treated in a HT-LSCM, where the formation of acicular ferrite is observable in situ. Finally, computerized metallographic analyses are applied to evaluate the fraction of acicular ferrite, prior austenite grain size and inclusion landscape. Using this methodology, the acicular ferrite formation in different steel grades is investigated extensively. Next to the determination of the optimum austenite grain size and suitable cooling rates, the effects of carbon, manganese, titanium, boron, chromium, nickel and magnesium are analysed. In addition, the thesis focuses on the evaluation of inclusions’ potential for acicular ferrite nucleation in the different steel grades. The findings of this work provide fundamental knowledge about the acicular ferrite formation and its main influencing factors, which is essential for the production of acicular ferritic steels on industrial scale.
AB - Acicular ferrite nucleates intragranularly on non-metallic inclusions, forming an arrangement of fine, interlocking grains. This characteristic structure is known to improve the steel toughness significantly, what makes acicular ferrite of increasing interest to steel producers. However, the formation of acicular ferrite is still not completely clarified. Therefore, the present thesis developed a holistic and systematic methodology to study the acicular ferrite formation and its influencing factors on laboratory scale. First, the necessary steel composition to create a desired inclusion landscape is determined by thermodynamic calculations using FactSage. Second, samples with defined and homogenously distributed inclusions are produced by melting experiments in a Tammann type furnace. The methodology only uses endogenous inclusions, resulting from deoxidation and desulphurization, as nucleation sites for acicular ferrite, so that the steel cleanness is not deteriorated artificially by the addition of synthetic particles. Third, the samples are heat treated in a HT-LSCM, where the formation of acicular ferrite is observable in situ. Finally, computerized metallographic analyses are applied to evaluate the fraction of acicular ferrite, prior austenite grain size and inclusion landscape. Using this methodology, the acicular ferrite formation in different steel grades is investigated extensively. Next to the determination of the optimum austenite grain size and suitable cooling rates, the effects of carbon, manganese, titanium, boron, chromium, nickel and magnesium are analysed. In addition, the thesis focuses on the evaluation of inclusions’ potential for acicular ferrite nucleation in the different steel grades. The findings of this work provide fundamental knowledge about the acicular ferrite formation and its main influencing factors, which is essential for the production of acicular ferritic steels on industrial scale.
KW - Acicular ferrite
KW - Non-metallic inclusions
KW - Microstructure
KW - FactSage
KW - HT-LSCM
KW - Azikularer Ferrit
KW - Nichtmetallische Einschlüsse
KW - Mikrostruktur
KW - FactSage
KW - HT-LSCM
M3 - Doctoral Thesis
ER -