Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Konferenzband

Standard

Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis. / Andreas, Frank; Bruckmoser, Katharina; Redhead, Anita et al.
Proceedings of "Austrian-Slovenian Polymer Meeting 2010". 2010. S. 145-145.

Publikationen: Beitrag in Buch/Bericht/KonferenzbandBeitrag in Konferenzband

Bibtex - Download

@inproceedings{9278249cc0aa44bfbdb7bdc8ed03befe,
title = "Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis",
author = "Frank Andreas and Katharina Bruckmoser and Anita Redhead and Gruber, {Dieter P.} and Gerald Pinter",
year = "2010",
language = "English",
pages = "145--145",
booktitle = "Proceedings of {"}Austrian-Slovenian Polymer Meeting 2010{"}",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis

AU - Andreas, Frank

AU - Bruckmoser, Katharina

AU - Redhead, Anita

AU - Gruber, Dieter P.

AU - Pinter, Gerald

PY - 2010

Y1 - 2010

M3 - Conference contribution

SP - 145

EP - 145

BT - Proceedings of "Austrian-Slovenian Polymer Meeting 2010"