Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Standard
Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis. / Andreas, Frank; Bruckmoser, Katharina; Redhead, Anita et al.
Proceedings of "Austrian-Slovenian Polymer Meeting 2010". 2010. p. 145-145.
Proceedings of "Austrian-Slovenian Polymer Meeting 2010". 2010. p. 145-145.
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Harvard
Andreas, F, Bruckmoser, K, Redhead, A, Gruber, DP & Pinter, G 2010, Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis. in Proceedings of "Austrian-Slovenian Polymer Meeting 2010". pp. 145-145.
APA
Andreas, F., Bruckmoser, K., Redhead, A., Gruber, D. P., & Pinter, G. (2010). Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis. In Proceedings of "Austrian-Slovenian Polymer Meeting 2010" (pp. 145-145)
Vancouver
Andreas F, Bruckmoser K, Redhead A, Gruber DP, Pinter G. Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis. In Proceedings of "Austrian-Slovenian Polymer Meeting 2010". 2010. p. 145-145
Author
Bibtex - Download
@inproceedings{9278249cc0aa44bfbdb7bdc8ed03befe,
title = "Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis",
author = "Frank Andreas and Katharina Bruckmoser and Anita Redhead and Gruber, {Dieter P.} and Gerald Pinter",
year = "2010",
language = "English",
pages = "145--145",
booktitle = "Proceedings of {"}Austrian-Slovenian Polymer Meeting 2010{"}",
}
RIS (suitable for import to EndNote) - Download
TY - GEN
T1 - Investigation of the slow crack growth behavior of static and cyclic loaded specimens of polyethylene by 2D and 3D optical fracture surface analysis
AU - Andreas, Frank
AU - Bruckmoser, Katharina
AU - Redhead, Anita
AU - Gruber, Dieter P.
AU - Pinter, Gerald
PY - 2010
Y1 - 2010
M3 - Conference contribution
SP - 145
EP - 145
BT - Proceedings of "Austrian-Slovenian Polymer Meeting 2010"
ER -