In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Standard
In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy. / Zickler, Gerald; Schnitzer, Ronald; Schweins, Ralf et al.
2008. Postersitzung präsentiert bei Deutsche Neutronenstreutagung 2008, Garching, Deutschland.
2008. Postersitzung präsentiert bei Deutsche Neutronenstreutagung 2008, Garching, Deutschland.
Publikationen: Konferenzbeitrag › Poster › Forschung › (peer-reviewed)
Harvard
Zickler, G, Schnitzer, R, Schweins, R & Leitner, H 2008, 'In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy', Deutsche Neutronenstreutagung 2008, Garching, Deutschland, 14/09/08 - 17/09/08.
APA
Zickler, G., Schnitzer, R., Schweins, R., & Leitner, H. (2008). In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy. Postersitzung präsentiert bei Deutsche Neutronenstreutagung 2008, Garching, Deutschland.
Vancouver
Zickler G, Schnitzer R, Schweins R, Leitner H. In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy. 2008. Postersitzung präsentiert bei Deutsche Neutronenstreutagung 2008, Garching, Deutschland.
Author
Bibtex - Download
@conference{f293593f5c4e4424827160fc78856c1e,
title = "In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy",
author = "Gerald Zickler and Ronald Schnitzer and Ralf Schweins and Harald Leitner",
year = "2008",
language = "English",
note = "Deutsche Neutronenstreutagung 2008 ; Conference date: 14-09-2008 Through 17-09-2008",
}
RIS (suitable for import to EndNote) - Download
TY - CONF
T1 - In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy
AU - Zickler, Gerald
AU - Schnitzer, Ronald
AU - Schweins, Ralf
AU - Leitner, Harald
PY - 2008
Y1 - 2008
M3 - Poster
T2 - Deutsche Neutronenstreutagung 2008
Y2 - 14 September 2008 through 17 September 2008
ER -