In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy

Research output: Contribution to conferencePosterResearchpeer-review

Standard

In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy. / Zickler, Gerald; Schnitzer, Ronald; Schweins, Ralf et al.
2008. Poster session presented at Deutsche Neutronenstreutagung 2008, Garching, Germany.

Research output: Contribution to conferencePosterResearchpeer-review

Harvard

Zickler, G, Schnitzer, R, Schweins, R & Leitner, H 2008, 'In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy', Deutsche Neutronenstreutagung 2008, Garching, Germany, 14/09/08 - 17/09/08.

APA

Zickler, G., Schnitzer, R., Schweins, R., & Leitner, H. (2008). In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy. Poster session presented at Deutsche Neutronenstreutagung 2008, Garching, Germany.

Vancouver

Zickler G, Schnitzer R, Schweins R, Leitner H. In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy. 2008. Poster session presented at Deutsche Neutronenstreutagung 2008, Garching, Germany.

Author

Zickler, Gerald ; Schnitzer, Ronald ; Schweins, Ralf et al. / In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy. Poster session presented at Deutsche Neutronenstreutagung 2008, Garching, Germany.

Bibtex - Download

@conference{f293593f5c4e4424827160fc78856c1e,
title = "In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy",
author = "Gerald Zickler and Ronald Schnitzer and Ralf Schweins and Harald Leitner",
year = "2008",
language = "English",
note = "Deutsche Neutronenstreutagung 2008 ; Conference date: 14-09-2008 Through 17-09-2008",

}

RIS (suitable for import to EndNote) - Download

TY - CONF

T1 - In-situ high-temperature characterization of intermetallic precipitates in a new nickel-based superalloy

AU - Zickler, Gerald

AU - Schnitzer, Ronald

AU - Schweins, Ralf

AU - Leitner, Harald

PY - 2008

Y1 - 2008

M3 - Poster

T2 - Deutsche Neutronenstreutagung 2008

Y2 - 14 September 2008 through 17 September 2008

ER -