Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Standard

Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten. / Goel, Saurav; Cross, Graham; Stukowski, Alexander et al.
in: Computational materials science, Jahrgang 152, 2018, S. 196-210.

Publikationen: Beitrag in FachzeitschriftArtikelForschung(peer-reviewed)

Vancouver

Goel S, Cross G, Stukowski A, Gamsjäger E, Beake B, Agrawal A. Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten. Computational materials science. 2018;152:196-210. doi: https://doi.org/10.1016/j.commatsci.2018.04.044

Author

Goel, Saurav ; Cross, Graham ; Stukowski, Alexander et al. / Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten. in: Computational materials science. 2018 ; Jahrgang 152. S. 196-210.

Bibtex - Download

@article{63c99d64ff454b1c9262a2af519b400e,
title = "Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten",
keywords = "MD simulation, Indenter, Nanoindentation, Deformation, Tungsten",
author = "Saurav Goel and Graham Cross and Alexander Stukowski and Ernst Gamsj{\"a}ger and Ben Beake and Anupam Agrawal",
year = "2018",
doi = "https://doi.org/10.1016/j.commatsci.2018.04.044",
language = "English",
volume = "152",
pages = "196--210",
journal = "Computational materials science",
issn = "0927-0256",
publisher = "Elsevier",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Designing nanoindentation simulation studies by appropriate indenter choices: Case study on single crystal tungsten

AU - Goel, Saurav

AU - Cross, Graham

AU - Stukowski, Alexander

AU - Gamsjäger, Ernst

AU - Beake, Ben

AU - Agrawal, Anupam

PY - 2018

Y1 - 2018

KW - MD simulation, Indenter, Nanoindentation, Deformation, Tungsten

U2 - https://doi.org/10.1016/j.commatsci.2018.04.044

DO - https://doi.org/10.1016/j.commatsci.2018.04.044

M3 - Article

VL - 152

SP - 196

EP - 210

JO - Computational materials science

JF - Computational materials science

SN - 0927-0256

ER -