Welding procedure for high strength welds and their microstructural evolution during solidification and cooling: IIW Doc. II-C-436-11
Research output: Non-textual form › Web publication/site › Research
Standard
Welding procedure for high strength welds and their microstructural evolution during solidification and cooling: IIW Doc. II-C-436-11. Vanovsek, Wolfgang (Author); Schnitzer, Ronald (Author); Schlagradl, Thomas (Author) et al.. 2012.
Research output: Non-textual form › Web publication/site › Research
Harvard
Vanovsek, W, Schnitzer, R, Schlagradl, T, Schneider, R, Posch, G, Schider, S, Bernhard, C, Leitner, H, Rauch, R, Fiedler, M & Stoschka, M, Welding procedure for high strength welds and their microstructural evolution during solidification and cooling: IIW Doc. II-C-436-11, 2012, Web publication/site. <http://www.iiwelding.org/sites/Commission-II/WUDocuments/II-1810r2-12.pdf>
APA
Vanovsek, W., Schnitzer, R., Schlagradl, T., Schneider, R., Posch, G., Schider, S., Bernhard, C., Leitner, H., Rauch, R., Fiedler, M., & Stoschka, M. (2012). Welding procedure for high strength welds and their microstructural evolution during solidification and cooling: IIW Doc. II-C-436-11. Web publication/site http://www.iiwelding.org/sites/Commission-II/WUDocuments/II-1810r2-12.pdf
Vancouver
Vanovsek W, Schnitzer R, Schlagradl T, Schneider R, Posch G, Schider S et al.. Welding procedure for high strength welds and their microstructural evolution during solidification and cooling: IIW Doc. II-C-436-11 2012.
Author
Bibtex - Download
@misc{d72ff1d83478467b83c4178162a6f9b0,
title = "Welding procedure for high strength welds and their microstructural evolution during solidification and cooling: IIW Doc. II-C-436-11",
author = "Wolfgang Vanovsek and Ronald Schnitzer and Thomas Schlagradl and Reinhold Schneider and Gerhard Posch and Siegfried Schider and Christian Bernhard and Harald Leitner and Rudolf Rauch and Michael Fiedler and Michael Stoschka",
year = "2012",
language = "English",
}
RIS (suitable for import to EndNote) - Download
TY - ADVS
T1 - Welding procedure for high strength welds and their microstructural evolution during solidification and cooling
T2 - IIW Doc. II-C-436-11
AU - Vanovsek, Wolfgang
AU - Schnitzer, Ronald
AU - Schlagradl, Thomas
AU - Schneider, Reinhold
AU - Posch, Gerhard
AU - Schider, Siegfried
AU - Bernhard, Christian
AU - Leitner, Harald
AU - Rauch, Rudolf
AU - Fiedler, Michael
AU - Stoschka, Michael
PY - 2012
Y1 - 2012
M3 - Web publication/site
ER -