Two different correlations between nanoindentation modulus and mineral content in the bone-cartilage interface
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
Details
Translated title of the contribution | Two different correlations between nanoindentation modulus and mineral content in the bone-cartilage interface |
---|---|
Original language | English |
Pages (from-to) | 138-148 |
Journal | Journal of structural biology |
Volume | 149 |
DOIs | |