The Effect of Surface Roughness on Nanoindentation of Hard Coatings: Simulation and Experiment
Research output: Contribution to conference › Poster › Research › peer-review
Authors
Organisational units
Details
Translated title of the contribution | The Effect of Surface Roughness on Nanoindentation of Hard Coatings: Simulation and Experiment |
---|---|
Original language | English |
Publication status | Published - 2009 |
Event | Nanomechanical Testing in Materials Research and Development - Barga, Italy Duration: 11 Oct 2009 → 16 Oct 2009 |