The deformation-induced zone below large and shallow nanoindentations: A comparative study using EBSD and TEM

Research output: Contribution to journalArticleResearchpeer-review

Authors

  • M. Rester
  • Christian Motz
  • Reinhard Pippan

Organisational units

Details

Translated title of the contributionThe deformation-induced zone below large and shallow nanoindentations: A comparative study using EBSD and TEM
Original languageEnglish
Pages (from-to)879-887
JournalPhilosophical magazine : Letters
Volume88
DOIs
Publication statusPublished - 2008