Studies on the melting behavior of polypropylene nano-composites using X-ray diffraction and differential scanning calorimetry
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Standard
ANTEC 2009 Society of Plastics Engineers' Annual Technical Conference. 2009. p. 2642-2646.
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - GEN
T1 - Studies on the melting behavior of polypropylene nano-composites using X-ray diffraction and differential scanning calorimetry
AU - Feuchter, Michael
AU - Maier, Günther
AU - Pinter, Gerald
AU - Kracalik, Milan
AU - Laske, Stephan
AU - Langecker, Günter
PY - 2009
Y1 - 2009
UR - http://www.scopus.com/inward/record.url?eid=2-s2.0-70450073191&partnerID=MN8TOARS
M3 - Conference contribution
SP - 2642
EP - 2646
BT - ANTEC 2009 Society of Plastics Engineers' Annual Technical Conference
ER -