Strain-induced martensitic transformation in a Co-Cr-W-Mo alloy probed by nanoindentation

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Standard

Strain-induced martensitic transformation in a Co-Cr-W-Mo alloy probed by nanoindentation. / Weißensteiner, Irmgard; Voigt, Patrick; Clemens, Helmut et al.
Proceedings of the International Conference on Martensitic Transformations. 2018. p. 247-250.

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Harvard

Weißensteiner, I, Voigt, P, Clemens, H & Maier-Kiener, V 2018, Strain-induced martensitic transformation in a Co-Cr-W-Mo alloy probed by nanoindentation. in Proceedings of the International Conference on Martensitic Transformations. pp. 247-250, International Conference on Martensitic Transformations 2017, Chicago, United States, 10/07/17. https://doi.org/10.1007/978-3-319-76968-4_38

Vancouver

Weißensteiner I, Voigt P, Clemens H, Maier-Kiener V. Strain-induced martensitic transformation in a Co-Cr-W-Mo alloy probed by nanoindentation. In Proceedings of the International Conference on Martensitic Transformations. 2018. p. 247-250 doi: 10.1007/978-3-319-76968-4_38

Author

Weißensteiner, Irmgard ; Voigt, Patrick ; Clemens, Helmut et al. / Strain-induced martensitic transformation in a Co-Cr-W-Mo alloy probed by nanoindentation. Proceedings of the International Conference on Martensitic Transformations. 2018. pp. 247-250

Bibtex - Download

@inproceedings{ce12de0fb97a4268820b76eab67d72db,
title = "Strain-induced martensitic transformation in a Co-Cr-W-Mo alloy probed by nanoindentation",
author = "Irmgard Wei{\ss}ensteiner and Patrick Voigt and Helmut Clemens and Verena Maier-Kiener",
year = "2018",
doi = "10.1007/978-3-319-76968-4_38",
language = "English",
pages = "247--250",
booktitle = "Proceedings of the International Conference on Martensitic Transformations",
note = "International Conference on Martensitic Transformations 2017 ; Conference date: 10-07-2017",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - Strain-induced martensitic transformation in a Co-Cr-W-Mo alloy probed by nanoindentation

AU - Weißensteiner, Irmgard

AU - Voigt, Patrick

AU - Clemens, Helmut

AU - Maier-Kiener, Verena

PY - 2018

Y1 - 2018

U2 - 10.1007/978-3-319-76968-4_38

DO - 10.1007/978-3-319-76968-4_38

M3 - Conference contribution

SP - 247

EP - 250

BT - Proceedings of the International Conference on Martensitic Transformations

T2 - International Conference on Martensitic Transformations 2017

Y2 - 10 July 2017

ER -