Quantum-mechanical study of tensorial elastic and high-temperature thermodynamic properties of grain boundary states in superalloy-phase Ni3Al
Research output: Contribution to journal › Article › Research › peer-review
Standard
In: IOP Conference Series: Materials Science and Engineering, Vol. 219.2017, 012019, 2017.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Quantum-mechanical study of tensorial elastic and high-temperature thermodynamic properties of grain boundary states in superalloy-phase Ni3Al
AU - Friák, Martin
AU - Vsianska, Monika
AU - Holec, David
AU - Šob, Mojmír
PY - 2017
Y1 - 2017
N2 - Grain boundaries (GBs), the most important defects in solids and their properties are crucial for many materials properties including (in-)stability. Quantum-mechanical methods can reliably compute properties of GBs and we use them to analyze (tensorial) anisotropic elastic properties of interface states associated with GBs in one of the most important intermetallic compounds for industrial applications, Ni3Al. Selecting the Σ5(210) GBs as a case study because of its significant extra volume, we address the mechanical stability of the GB interface states by checking elasticity-based Born stability criteria. One critically important elastic constant, C55, is found nearly three times smaller at the GB compared with the bulk, contributing thus to the reduction of the mechanical stability of Ni3Al polycrystals. Next, comparing properties of Σ5(210) GB state which is fully relaxed with those of a Σ5(210) GB state when the supercell dimensions are kept equal to those in the bulk we conclude that lateral relaxations have only marginal impact on the studied properties. Having the complete elastic tensor of Σ5(210) GB states we combine Green's-function based homogenization techniques and an approximative approach to the Debye model to compare thermodynamic properties of a perfect Ni3Al bulk and the Σ5(210) GB states. In particular, significant reduction of the melting temperature (to 79-81% of the bulk value) is predicted for nanometer-size grains.
AB - Grain boundaries (GBs), the most important defects in solids and their properties are crucial for many materials properties including (in-)stability. Quantum-mechanical methods can reliably compute properties of GBs and we use them to analyze (tensorial) anisotropic elastic properties of interface states associated with GBs in one of the most important intermetallic compounds for industrial applications, Ni3Al. Selecting the Σ5(210) GBs as a case study because of its significant extra volume, we address the mechanical stability of the GB interface states by checking elasticity-based Born stability criteria. One critically important elastic constant, C55, is found nearly three times smaller at the GB compared with the bulk, contributing thus to the reduction of the mechanical stability of Ni3Al polycrystals. Next, comparing properties of Σ5(210) GB state which is fully relaxed with those of a Σ5(210) GB state when the supercell dimensions are kept equal to those in the bulk we conclude that lateral relaxations have only marginal impact on the studied properties. Having the complete elastic tensor of Σ5(210) GB states we combine Green's-function based homogenization techniques and an approximative approach to the Debye model to compare thermodynamic properties of a perfect Ni3Al bulk and the Σ5(210) GB states. In particular, significant reduction of the melting temperature (to 79-81% of the bulk value) is predicted for nanometer-size grains.
U2 - 10.1088/1757-899X/219/1/012019
DO - 10.1088/1757-899X/219/1/012019
M3 - Article
VL - 219.2017
JO - IOP Conference Series: Materials Science and Engineering
JF - IOP Conference Series: Materials Science and Engineering
SN - 1757-899X
M1 - 012019
ER -