δ-Phase characterization of superalloy allvac 718 PlusTM

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Authors

  • C. Stotter
  • S. Mitsche
  • I. Letofsky-Papst
  • M. Stockinger

Details

Translated title of the contributionδ-Phase characterization of superalloy allvac 718 PlusTM
Original languageEnglish
Title of host publicationTMS 2008
Pages1-6