Nanoindentation of regenerated cellulose fibres

Research output: Contribution to journalArticleResearchpeer-review

Authors

  • W. Gindl
  • J. Konnerth
  • Thomas Schöberl

Organisational units

Details

Translated title of the contributionNanoindentation of regenerated cellulose fibres
Original languageEnglish
Pages (from-to)1-7
JournalCellulose
Volume13