Modeling and Investigation of Dynamic Recrystallisation in Nickel-Based Superalloys
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
Details
Translated title of the contribution | Modeling and Investigation of Dynamic Recrystallisation in Nickel-Based Superalloys |
---|---|
Original language | English |
Pages (from-to) | 743-748 |
Journal | Materials Science Forum |
Publication status | Published - 2003 |