Microstructure modeling of the dynamic recrystallization kinetics during turbine disc forging of the nickel based superalloy Allvac 718PlusTM
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Authors
Organisational units
Details
Translated title of the contribution | Microstructure modeling of the dynamic recrystallization kinetics during turbine disc forging of the nickel based superalloy Allvac 718PlusTM |
---|---|
Original language | English |
Title of host publication | Superalloys 2008, Roger C. Reed et al. Eds., TMS |
Pages | 855-861 |