Microstructural investigation of thermally aged nickel-based superalloy 718Plus

Research output: Contribution to journalArticleResearchpeer-review

Authors

  • Mohammed Reza Ahmadi
  • Martin Stockinger
  • Erwin Povoden-Karadeniz
  • Ernst Kozeschnik

Details

Translated title of the contributionMicrostructural investigation of thermally aged nickel-based superalloy 718Plus
Original languageEnglish
Pages (from-to)253-259
JournalMaterials science and engineering: A, Structural materials: properties, microstructure and processing
Volume594
DOIs
Publication statusPublished - 2014