Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Standard

Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper. / Rester, M.; Motz, Christian; Pippan, Reinhard.
Materials Research Society. Materials Research Society : MRS, 2008. p. 1049-1055.

Research output: Chapter in Book/Report/Conference proceedingConference contribution

Harvard

Rester, M, Motz, C & Pippan, R 2008, Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper. in Materials Research Society. Materials Research Society : MRS, pp. 1049-1055.

APA

Rester, M., Motz, C., & Pippan, R. (2008). Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper. In Materials Research Society (pp. 1049-1055). Materials Research Society : MRS.

Vancouver

Rester M, Motz C, Pippan R. Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper. In Materials Research Society. Materials Research Society : MRS. 2008. p. 1049-1055

Author

Rester, M. ; Motz, Christian ; Pippan, Reinhard. / Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper. Materials Research Society. Materials Research Society : MRS, 2008. pp. 1049-1055

Bibtex - Download

@inproceedings{0cba02ebdde542c0a9fc4205ccb334a4,
title = "Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper",
author = "M. Rester and Christian Motz and Reinhard Pippan",
year = "2008",
language = "English",
pages = "1049--1055",
booktitle = "Materials Research Society",
publisher = "Materials Research Society : MRS",
address = "United States",

}

RIS (suitable for import to EndNote) - Download

TY - GEN

T1 - Microstructural Investigation of the Deformation Zone below Nano-Indents in Copper

AU - Rester, M.

AU - Motz, Christian

AU - Pippan, Reinhard

PY - 2008

Y1 - 2008

M3 - Conference contribution

SP - 1049

EP - 1055

BT - Materials Research Society

PB - Materials Research Society : MRS

ER -