Microstructural characterization of a double pulse resistance spot welded 1200 Mpa TBF steel
Research output: Contribution to journal › Article › Research › peer-review
Standard
In: Welding in the world, Vol. 64.2020, No. 2, 01.02.2020, p. 335-343.
Research output: Contribution to journal › Article › Research › peer-review
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - JOUR
T1 - Microstructural characterization of a double pulse resistance spot welded 1200 Mpa TBF steel
AU - Stadler, Manfred
AU - Gruber, Martin
AU - Schnitzer, Ronald
AU - Hofer, Christina
N1 - Publisher Copyright: © 2019, The Author(s).
PY - 2020/2/1
Y1 - 2020/2/1
N2 - In the automotive industry resistance, spot welding is the dominant technology in sheet metal joining of advanced high strength steels (AHSS). In order to improve the mechanical performance of AHSS welds, in-process tempering via a second pulse is a possible approach. In this work, two different double pulse welding schemes were applied to a 1200 MPa transformation-induced plasticity (TRIP)-aided bainitic ferrite (TBF) steel. The different microstructures in the welds were characterized via light optical and scanning electron microscopy. Additionally, hardness mappings with several hundred indents were performed. It is shown that the second pulse, following a low first pulse which is high enough to produce a weld nugget that fulfills the quality criterion of a minimum spot weld diameter of 4*√t, leads to partial reaustenitization and consequently to a ferritic/martensitic microstructure after final quenching. Hardness mappings revealed that this inner FZ is harder than the surrounding FZ consisting of tempered martensite. In contrast, if the highest current without splashing is chosen for the first pulse, the same second pulse does not reaustenitize the FZ but only temper the martensite.
AB - In the automotive industry resistance, spot welding is the dominant technology in sheet metal joining of advanced high strength steels (AHSS). In order to improve the mechanical performance of AHSS welds, in-process tempering via a second pulse is a possible approach. In this work, two different double pulse welding schemes were applied to a 1200 MPa transformation-induced plasticity (TRIP)-aided bainitic ferrite (TBF) steel. The different microstructures in the welds were characterized via light optical and scanning electron microscopy. Additionally, hardness mappings with several hundred indents were performed. It is shown that the second pulse, following a low first pulse which is high enough to produce a weld nugget that fulfills the quality criterion of a minimum spot weld diameter of 4*√t, leads to partial reaustenitization and consequently to a ferritic/martensitic microstructure after final quenching. Hardness mappings revealed that this inner FZ is harder than the surrounding FZ consisting of tempered martensite. In contrast, if the highest current without splashing is chosen for the first pulse, the same second pulse does not reaustenitize the FZ but only temper the martensite.
UR - http://www.scopus.com/inward/record.url?scp=85076528367&partnerID=8YFLogxK
U2 - 10.1007/s40194-019-00835-9
DO - 10.1007/s40194-019-00835-9
M3 - Article
VL - 64.2020
SP - 335
EP - 343
JO - Welding in the world
JF - Welding in the world
SN - 0043-2288
IS - 2
ER -