Mechanical properties of pyrolysed wood: a nanoindentation study
Research output: Contribution to journal › Article › Research › peer-review
Authors
Organisational units
Details
Translated title of the contribution | Mechanical properties of pyrolysed wood: a nanoindentation study |
---|---|
Original language | English |
Pages (from-to) | 1373-1386 |
Journal | Philosophical magazine |
Volume | 86 |
Publication status | Published - 2006 |