Investigation of Refractory Brittleness by Fracture Mechanical and Fractographic Methods

Research output: Contribution to journalArticleResearchpeer-review

Standard

Investigation of Refractory Brittleness by Fracture Mechanical and Fractographic Methods. / Harmuth, Harald; Bradt, Richard C.
In: Interceram / Refractories manual, 2010, p. 6-10.

Research output: Contribution to journalArticleResearchpeer-review

Bibtex - Download

@article{11c5da19385c459597fc37f2c484c84d,
title = "Investigation of Refractory Brittleness by Fracture Mechanical and Fractographic Methods",
author = "Harald Harmuth and Bradt, {Richard C.}",
year = "2010",
language = "English",
pages = "6--10",
journal = "Interceram / Refractories manual",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Investigation of Refractory Brittleness by Fracture Mechanical and Fractographic Methods

AU - Harmuth, Harald

AU - Bradt, Richard C.

PY - 2010

Y1 - 2010

M3 - Article

SP - 6

EP - 10

JO - Interceram / Refractories manual

JF - Interceram / Refractories manual

ER -