In-situ study of the dissolution of SiO2 inclusions in secondary steelmaking slags for the production of steel wire
Research output: Thesis › Master's Thesis
Standard
2013. 89 p.
Research output: Thesis › Master's Thesis
Harvard
APA
Vancouver
Author
Bibtex - Download
}
RIS (suitable for import to EndNote) - Download
TY - THES
T1 - In-situ study of the dissolution of SiO2 inclusions in secondary steelmaking slags for the production of steel wire
AU - Feichtinger, Stefan
N1 - embargoed until null
PY - 2013
Y1 - 2013
N2 - Non-metallic inclusions are the main reason for steel wire breakage of highly demanding products like tire cord. Therefore efficient removal of non-metallic inclusions by top slags needs to be ensured. The present thesis deals with the dissolution behaviour of SiO2 in different slags. The first part of the present thesis gives an overview of the state of the art of inclusion control during the production of steel wires and of inclusion dissolution studies. The present work is the first to study the dissolution of SiO2 inclusions in steelmaking slags by high temperature-confocal scanning laser microscopy. Scatter of the measurements was reduced by using spherical glassy silica inclusions in the experiments. SEM-EDS analysis and calculation of the relevant phase diagram showed that reaction layers around the particle are not formed during the dissolution which allowed the focus to be kept on the dissolution mechanism. For the first time it was observed that the dissolution mechanism changes as a function of the slag composition. The slag viscosity can be identified as the main influence on reaction mechanism and dissolution time. A new adapted model based on approximations of the diffusion equation which allows the interpretation of changing reaction mechanisms is introduced. Moreover the SiO2 diffusion coefficients are calculated and a regression model for the prediction of the dissolution time of SiO2 in a low alumina slag is presented.
AB - Non-metallic inclusions are the main reason for steel wire breakage of highly demanding products like tire cord. Therefore efficient removal of non-metallic inclusions by top slags needs to be ensured. The present thesis deals with the dissolution behaviour of SiO2 in different slags. The first part of the present thesis gives an overview of the state of the art of inclusion control during the production of steel wires and of inclusion dissolution studies. The present work is the first to study the dissolution of SiO2 inclusions in steelmaking slags by high temperature-confocal scanning laser microscopy. Scatter of the measurements was reduced by using spherical glassy silica inclusions in the experiments. SEM-EDS analysis and calculation of the relevant phase diagram showed that reaction layers around the particle are not formed during the dissolution which allowed the focus to be kept on the dissolution mechanism. For the first time it was observed that the dissolution mechanism changes as a function of the slag composition. The slag viscosity can be identified as the main influence on reaction mechanism and dissolution time. A new adapted model based on approximations of the diffusion equation which allows the interpretation of changing reaction mechanisms is introduced. Moreover the SiO2 diffusion coefficients are calculated and a regression model for the prediction of the dissolution time of SiO2 in a low alumina slag is presented.
KW - non-metallic inclusions
KW - silica
KW - SiO2
KW - wire
KW - tire cord
KW - confocal microscope
KW - dissolution
KW - slags
KW - low alumina
KW - dissolution mechanism
KW - diffusion
KW - nichtmetallische Einschlüsse
KW - SiO2
KW - Draht
KW - Stahlcord
KW - Konfokalmikroskop
KW - Auflösung
KW - Schlacken
KW - Auflösungsmechanismus
M3 - Master's Thesis