Influence of severe straining and strain rate on the evolution of dislocation structures during micro-/nanoindentation in high entropy lamellar eutectics

Research output: Contribution to journalArticleResearchpeer-review

Standard

Influence of severe straining and strain rate on the evolution of dislocation structures during micro-/nanoindentation in high entropy lamellar eutectics. / Maity, Tapabrata; Prashanth, Konda Gokuldoss; Balci, Özge et al.
In: International journal of plasticity, Vol. 109.2018, No. October, 31.05.2018, p. 121-136.

Research output: Contribution to journalArticleResearchpeer-review

Vancouver

Maity T, Prashanth KG, Balci Ö, Kim JT, Schöberl T, Wang Z et al. Influence of severe straining and strain rate on the evolution of dislocation structures during micro-/nanoindentation in high entropy lamellar eutectics. International journal of plasticity. 2018 May 31;109.2018(October):121-136. Epub 2018 May 31. doi: 10.1016/j.ijplas.2018.05.012

Bibtex - Download

@article{9d7f966c17e1456aa2781681a403d9df,
title = "Influence of severe straining and strain rate on the evolution of dislocation structures during micro-/nanoindentation in high entropy lamellar eutectics",
keywords = "Deformation mechanism, Dislocations, Eutectic high entropy alloys, Micro-/nanoindentation, Plasticity, Strengthening mechanism",
author = "Tapabrata Maity and Prashanth, {Konda Gokuldoss} and {\"O}zge Balci and Kim, {Jeong Tae} and Thomas Sch{\"o}berl and Zhi Wang and J{\"u}rgen Eckert",
year = "2018",
month = may,
day = "31",
doi = "10.1016/j.ijplas.2018.05.012",
language = "English",
volume = "109.2018",
pages = "121--136",
journal = "International journal of plasticity",
issn = "0749-6419",
publisher = "Elsevier Ltd",
number = "October",

}

RIS (suitable for import to EndNote) - Download

TY - JOUR

T1 - Influence of severe straining and strain rate on the evolution of dislocation structures during micro-/nanoindentation in high entropy lamellar eutectics

AU - Maity, Tapabrata

AU - Prashanth, Konda Gokuldoss

AU - Balci, Özge

AU - Kim, Jeong Tae

AU - Schöberl, Thomas

AU - Wang, Zhi

AU - Eckert, Jürgen

PY - 2018/5/31

Y1 - 2018/5/31

KW - Deformation mechanism

KW - Dislocations

KW - Eutectic high entropy alloys

KW - Micro-/nanoindentation

KW - Plasticity

KW - Strengthening mechanism

UR - http://www.scopus.com/inward/record.url?scp=85048242191&partnerID=8YFLogxK

U2 - 10.1016/j.ijplas.2018.05.012

DO - 10.1016/j.ijplas.2018.05.012

M3 - Article

AN - SCOPUS:85048242191

VL - 109.2018

SP - 121

EP - 136

JO - International journal of plasticity

JF - International journal of plasticity

SN - 0749-6419

IS - October

ER -