Influence of Cold Deformation on Stress Corrosion Cracking Resistance of Highly Alloyed Austenitic Stainless Steels in Chloride Media
Research output: Chapter in Book/Report/Conference proceeding › Conference contribution
Authors
Organisational units
Details
Translated title of the contribution | Influence of Cold Deformation on Stress Corrosion Cracking Resistance of Highly Alloyed Austenitic Stainless Steels in Chloride Media |
---|---|
Original language | English |
Title of host publication | Proceedings of the Corrosion 2006 |
Publisher | Omnipress |
Pages | 1-17 |
Publication status | Published - 2006 |